However, after about 20 hours, the anodic film thickness decreased sufficiently to allow the faradaic processes toinerease to, the final steady state value.
Anionic electrodeposit coating line for aluminum shell of solar water heater is introduced.Anodic oxidation,anodizing electrolytic coloring and anionic electrodeposit coating process are focused.
The selective oxidation of ethers by chromic reagent, peroxide, nitric acid, oxygen and ozonide, as well as the ethers anodic oxidation are particularly introduced.