The test results showed that the Mooney viscosity,mixing behavior and curing rate increased,and the filtering and extrudability improved by blending EPDM and an elastic filler in the test compound.
试验配方中并用EPDM和弹性填充,门尼粘度、硫化速度和混炼性得到提高,过滤和挤出艺性得到改善。采用试验配方生产的自行车内胎性,达到国家标准要求;